u/flyer_kaz

Image 1 — W2 kiritsuke quench question.
Image 2 — W2 kiritsuke quench question.

W2 kiritsuke quench question.

Hey all! Got a W2 from NJ Steel Baron that I’ve ground and it’s ready for HT. I’ve made one before and it came out pretty good for my first time doing a hamon on W2.

My question is, I’m looking to get a little more detail and activity out of the hamon this go around and I know I can do an interrupted quench in water or brine first for like 2-3 seconds and then into the oil, but obviously my concern is with cracking. So with that in mind, has anyone done a quench in cooled oil for a happy medium with less worry about cracking from the water?

Would love everyone’s input if you’ve tried this or from any of the material autists. lol

Cheers!

Kaz