Hi everyone,

I'm getting tree supports crumbling into small debris mid-print on my Bambu H2D + 0.2 mm nozzle at 0.08 mm layer height (also tried 0.06mm). In my last print central parts fail with blobs/stringing while sides print fine (see video)

Current profile with what is changed or important from bambu default

Quality

  • Layer height: 0.08 mm
  • Wall generator: Classic
  • Precision: Slice gap 0.001 / Resolution 0.001
  • Avoid crossing wall + support: ON

Speed

  • Outer Wall : 50 mm/s
  • Inner Wall : 50 mm/s
  • Support : 40 mm/s
  • Travel : 500 mm/s
  • Top Surface : 50 mm/s
  • Bridge : 15 mm/s
  • Initial Layer : 25 mm/s
  • Overhang Speed : Activé (30 / 25 / 15 / 5 / 5 mm/s selon les %)

Accelerations

  • Normal printing : 3000 mm/s²
  • Travel : 5000 mm/s²
  • Outer Wall : 2500 mm/s²
  • Initial Layer : 250 mm/s²
  • Top Surface : 500 mm/s²

Supports

  • Type: Tree (Auto)
  • Base Pattern: Rectilinear
  • Base Pattern Spacing: 1.6 mm
  • Top Z Distance: 0.18 mm
  • Tree Support: Branch diameter 2 mm / Branch angle 60°
  • Support Line Width: 0.28 mm
  • Brim: 9 mm

Other / Calibrations

  • Wall loops: 4
  • Infill: 25% Gyroid
  • Bambu glue stick for bed adhesion
  • Flow calibration + Dynamic Flow Calibration done (K=0.02)
  • Z-hop: 0.6 mm with spiral travel

Questions

I am a bit lost to what I should do or test actually, already read some messages from this subreddit, this is why I increased Z-hop or activated avoid crossing walls, with those I got from supports always knocked to support breacking but I can go further on my prints in general. On 0.4mm nozzle I have no issues at all. I have 3 different 0.2 nozzles that I tried to be sure this was not nozzle related. Any help appreciated :)