u/Cautious-Link1691

Image 1 — Tried 20V on 14 ga stainless
Image 2 — Tried 20V on 14 ga stainless
Image 3 — Tried 20V on 14 ga stainless

Tried 20V on 14 ga stainless

Bumped the volts up to 20 this time to see what happens.

Settings: Yeswelder DP200, 100A / 20.0V, 0.030" wire, 14 Ga stainless, 2T, 348 IPM wire speed, 98/2 Ar-CO2.

Honestly looks worse than before lol.
Face and backside pics attached. What am I doing wrong?

u/Cautious-Link1691 — 1 day ago

14 Ga stainless T-joint with C2 mix. Honest opinions?

Took the sub's advice and switched from straight argon to 98/2 Ar-CO2.

Settings: Yeswelder DP200, 100A / 18.5V, 0.030" wire, 14 Ga stainless, 2T, ~8.8 MPM wire speed.

Face side looks way nicer to me, way less of that wide heat tint. Back side is actually presentable now too.

Face and backside pics attached. How's it looking now? Anything else I should tweak?

u/Cautious-Link1691 — 2 months ago

3.2mm stainless butt. Honest opinions?

Hobbyist here. Been running a Yeswelder DP200 for a while. Threw together a 3.2mm stainless butt joint in the garage.

Settings: 100A/18.5V, 0.8mm wire, 98% argon.

Face side cleaned up okay, but there's some heat tint around the bead. Not sure if that's normal or if I'm doing something wrong, too much heat input or moving too slow?

Any feedback would be welcomed. Detailed Settings in last pic.

u/Cautious-Link1691 — 3 months ago