Hey everyone,

It's my first time printing Petg and my print shows these lines, I've dried the fillement on 60 C for 24 hours. Is this still a moisture issue, or a potential setting/printer issue? Weirdly enough the layers higher up don't have the same issue

Printed on bambu lab A1 mini using bambu lab petg HF. 0.4mm hardened nozzle

Slicer bambu studio,

System preset: 0.2mm standard @BBL A1M

Nozzle temp 245

Bed temp 70

It's a shower shelf so it doesn't have to be perfect, was just wondering what I could do to make it better.

Any tips and suggestions are more than welcome! Thanks in advance!