u/frugmonkey

Image 1 — Am I screwed (again)
Image 2 — Am I screwed (again)

Am I screwed (again)

48 hours in, and my resin is still tacky/soft on some areas of the roof, annoyingly this is the 2nd attempt to get the top layer looking right, the first attempt ended up with some cloudy looking patches in the resin which were visible under bright light (I think these were sanding marks which the following coats of resin didn't fill in properly)

I've had a heater under it since I put the first coat of resin on, but it's still not curing, I'm gonna leave it cooking overnight in the hope it goes off, but it not looking good.

Is there anything I can do to help it along?I don't want to risk sanding yet it in case it does the same thing as last time.

Resin is easy composites EL2, with a 50/50 mix of fast and slow hardener, I'm pretty sure it was well mixed (I did each cup for 5 minutes, scraping the sides/bottom and stirrer as I went

u/frugmonkey — 2 days ago