u/Far_Detective9205

Image 1 — Aluminum TIG in 3F has me by the balls
Image 2 — Aluminum TIG in 3F has me by the balls
Image 3 — Aluminum TIG in 3F has me by the balls
Image 4 — Aluminum TIG in 3F has me by the balls
Image 5 — Aluminum TIG in 3F has me by the balls
▲ 17 r/Welders

Aluminum TIG in 3F has me by the balls

Going on 5 days trying to get a testable T- joint . Haven’t been able to get into a good rhythm. I notice it’s difficult to focus the arc and I’m getting burn thru 80% of the time. Got through steel and stainless pretty quick. Aluminum 2G and 3G were cake but T-joint aren’t it for me. Any tips and advice would be helpful.